Cold and hot forming of Inconel alloy 600 is possible with conventional techniques. Because the ductility declines between 1200- and 1600-degrees Fahrenheit, hot work should only be done between 1600- and 2250-degrees Fahrenheit. Moreover, SMA, TIG, and MIG are all acceptable methods for welding alloy 600. Inconel 600 Basics Description […]